Why is design life not service life?
AEC's AGM VRLA blocks have a design life of 10 to 12 years by the EUROBAT guide. That figure assumes 25 °C (77 °F). A common rule of thumb says VRLA life halves for about every 8 °C (14 °F) above that: a block designed for 10 years lasts about 5 in a room at 33 °C (91 °F). The batteries page lets you slide the temperature and see it.
How much does a warm room take away?
The halving rule gives the life at any temperature: life = design life × 0.5(T − 77 °F) ÷ 15. For a block designed for 10 years:
| Room temperature | Expected life | Replacements in 15 years |
|---|---|---|
| 77 °F (25 °C) | about 10 years | 1 |
| 86 °F (30 °C) | about 6.6 years | 2 |
| 95 °F (35 °C) | about 4.4 years | 3 |
The rule is an approximation, not a promise, but the direction is certain: a closet without cooling, a UPS against a hot wall or a battery cabinet beside the exhaust of a server rack loses years. A thermometer at the battery, not at the room's thermostat, tells the truth.
How do outages and cycles wear a battery?
Every discharge and recharge is a cycle, and deep cycles wear a battery more than shallow ones. A UPS in a city with a stable grid may see a handful of short events a year; one at the end of a long rural line, or on a site that tests on battery every week, sees many more. Lead-acid is the more sensitive: a general-purpose 12 V 9 Ah AGM block is designed for about 300 cycles, where LUMINA's lithium is rated for 3,000 and the L6 cabinets for more than 5,000.
When is a battery at the end of its life?
By the usual definition, when its capacity has fallen to 80 % of its rating: IEEE 1188, the US recommended practice for VRLA batteries, uses that point for replacement. The runtime falls with the capacity, so a UPS that met its minutes on day one with no margin will not meet them at the end. Two ways to plan for it: size the battery so the minutes needed are still there at 80 % capacity, and test the battery every year so the end is seen before an outage finds it. When the time comes, the battery replacement tool gives the block in every AEC UPS and cabinet, and how many.
How long does lithium iron phosphate last?
- LUMINA: internal LiFePO4 rated for 12 to 15 years and 3,000 cycles, with about 2.6 times the full-load runtime of the VRLA FERRUS RT of the same rating at 1, 2 and 3 kVA (11 against 4.2 min), about 1.8 times at 1.5 kVA (11 against 6 min), each at its own full load (from the catalog's runtime tables).
- L6 lithium cabinets for large systems: 15 years and over 5,000 cycles.
- ETHERNO: 50 Ah lithium modules that come out and go in without shutting the load down, five-year warranty with the batteries included.
Over the life of a UPS, that usually means fewer battery replacements with lithium than with VRLA, less weight on the floor and less cooling. The L6 lithium page shows them on AEC cabinets.
Which battery does each AEC series use?
| Series | Battery | Battery warranty |
|---|---|---|
| LUMINA | Internal LiFePO4 | 5 years, with the UPS |
| ETHERNO | Hot-swappable 50 Ah LiFePO4 modules, 15-year module life | 5 years, with the UPS |
| FERRUS, FERRUS RT, FERRUS SP | Internal 12 V 9 Ah VRLA, external packs and cabinets for more runtime | 2 years |
| FERRUS SP RT | External 3U rack cabinets of 16 × 12 V 9 Ah VRLA (BAT16192RT) | 2 years |
| AUREON | Internal hot-swappable 12 V 9 Ah VRLA, up to 80 blocks (20, 40, 60 or 80) | 2 years |
| RADIANT-IB, CIRRO-IB | Up to 240 internal 12 V 9 Ah VRLA blocks in hot-swappable trays | 2 years |
| RADIANT, CIRRO | External VRLA bank | 2 years |
| INFINITE, INFINITE 1.5MW | External L6 lithium cabinets or lead-acid | 5 years on the L6 cabinets |
The UPS warranties are separate: five years on LUMINA and ETHERNO, three on the other series, five on INFINITE when registered.
What are the signs a battery is near its end?
- The UPS battery test fails, or the runtime at the same load is clearly shorter than at commissioning.
- VRLA blocks that are swollen, hot or leaking.
- Blocks in one string that read very different voltages or internal resistance.
What good practice makes batteries last?
- Keep the battery room near 25 °C (77 °F): it is the single biggest factor in VRLA life.
- Replace every block in a string together; one new block among old ones ages with them.
- Let a specialist test and change the batteries, with the charger settings the maker gives.
- Recycle lead-acid blocks through a battery recycler; they are fully recyclable.
- Use high-rate UPS blocks. AEC's published runtimes are based on high-rate cells; a general-purpose block of the same size gives fewer minutes at UPS loads and fewer cycles.
- Keep a UPS that sits unused on charge, or recharge it at the interval its manual gives: a stored battery loses charge, and a VRLA block left flat sulfates.
- Write the installation date on the cabinet and in the maintenance log, so the replacement is planned, not discovered.
AEC sells 12 V VRLA blocks loose for battery cabinets and for replacing the blocks inside a UPS.